I. Stern 108B Utility Black ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer I. Stern & Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern 108B Utility Black ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Good processing characteristicsInjection Molding and ExtrusionApplicationsProfilesPicture Frames, Tubes, RodsSpools, ReelsInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched >= 1.33 J/cm
>= 2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 98.9 °C
210 °F
ASTM D1525