Hyosung Topilene R701G PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene R701G PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
R701G Random CopolymerApplications:Disposable syringeGamma-ray sterilizationCharacteristics:Gamma-ray resistancyHigh transparencyInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 26 g/10 min
26 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.13 GPa
164 ksi
ASTM D790
Izod Impact, Unnotched 0.588 J/cm
1.10 ft-lb/in
ASTM D256