Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene R701 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
R701 Injection Random CopolymerApplications:High transparent productISBM bottleCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 30.4 MPa
4410 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.13 GPa
164 ksi
ASTM D790
Izod Impact, Unnotched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %