Material Notes:
J700-1 Injection Special Purpose GradeApplications:Disposable syringeHouseware applianceCharacteristics:Slip propertyHigh stiffnessFast cycleInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 39.2 MPa
5690 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Unnotched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525