Hyosung Topilene HB242P PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene HB242P PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HB242P Applications:Industrial pipesSewerage pipesCharacteristics:High impact strengthHigh ring stiffnessInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 0.30 g/10 min
0.30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Unnotched 5.39 J/cm
10.1 ft-lb/in
ASTM D256
0.686 J/cm

@Temperature -10.0 °C
1.29 ft-lb/in

@Temperature 14.0 °F
ASTM D256