Material Notes:
POSS® Flow masterbatches show success in reducing the melt viscosity of a variety of injection molded and extruded resins. Hybrid Plastics now introduces such a solution for polyamide polymers. Polyamide POSS® Flow is a pellet masterbatch incorporating POSS® that can be used directly in the process or manufacturing stream. For injection molding applications, benefits include decreased molding pressures and increased flow for filling intricate and thin-walled parts. This leads to faster cycle times and less scrap. For extrusion applications, POSS® Flow decreases screw torque, allowing increased extrusion rates.At loading levels of up to 10%, Polyamide POSS® Flow does not significantly affect mechanical properties such as modulus, yield strength, or elongation to break. At a 20% loading, there is only a minor decrease in modulus and yield strength.This product is offered in two different versions. Polyamide POSS® Flow is for use in systems without particles or fillers. Polyamide POSS® Flow with POSS® Dispersant combines two POSS technologies into one product. POSS® Flow decreases melt viscosity, while POSS® Dispersant coats and disperses particles reducing melt viscosity even further, thereby increasing productivity and allowing up to three times as much filler to be added.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Filler Content 10 - 20 %
10 - 20 %
Melt Flow 110 g/10 min

@Load 2.16 kg,
Temperature 180 °C
110 g/10 min

@Load 4.76 lb,
Temperature 356 °F
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
Decomposition Temperature 350 °C
662 °F
5% wt loss in N<sub>2</sub>
Descriptive Properties Value Comments
Color translucent, light brown
Users viewing this material also viewed the following: