Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman Rexell® L2102 Injection Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Rexell® L2102 Injection Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear low density copolymer, injection molding, FDA compliant.Features: High flow, medium flex with good environmental stress crack (ESCR), and warpage resistance.Applications: Fitments, large lids, articles requiring extremely long flow paths, and low warpage.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2.aInformation provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Viscosity 50 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
50 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
90 cP

@Shear Rate 1000 1/s,
Temperature 230 °C
90 cP

@Shear Rate 1000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
140 cP

@Shear Rate 300 1/s,
Temperature 230 °C
140 cP

@Shear Rate 300 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Melt Flow 24 g/10 min
24 g/10 min
Melt Flow Ratio (I10/I2) is 7.4; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Modulus of Elasticity 0.320 GPa
46.4 ksi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 96.0 °C
205 °F
ASTM D1525