Huntsman PE7076 Profile Extrusion Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Sheet/Profile extrusions
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman PE7076 Profile Extrusion Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer and FDA compliant.Features: Yields parts with high gloss and excellent stiffness.Applications: Extrusion: profile extrusion.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 14.0 MPa
2030 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Modulus of Elasticity 0.483 GPa
70.1 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C
225 °F
ASTM D1525