Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman PE2051 Injection Molding Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman PE2051 Injection Molding Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer and FDA compliant.Features: Very good molding processability, produces parts with good stiffness, and shows excellent flatness in large projected areas. Also recommended for multi-cavity, fast cycle products, and low melt temperature.Applications: Injection molding: housewares, industrial parts, and general purpose molding where improved gloss and stiffness is required.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Modulus of Elasticity 0.449 GPa
65.1 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Users viewing this material also viewed the following: