Huntsman Kerimid 701-1 B US Resin

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Kerimid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Kerimid 701-1 B US Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Comments/Applications: Used with Kerimid 701 A US for high Tg laminate systems. Suggested ratio 3 parts A to 1 part B.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 20 - 80 cP
20 - 80 cP