Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman IROGRAN® A 98 P 4535 TPU-Polyether

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® A 98 P 4535 TPU-Polyether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D995
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength at Break 55.0 MPa
7980 psi
DIN 53504
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.0154 GPa
2.23 ksi
DIN 53504
300% Modulus 0.0250 GPa
3.63 ksi
DIN 53504
Rebound 30 %
30 %
Bayshore; ASTM D2632
Tear Strength 147 kN/m
840 pli
ASTM D624
Abrasion 30
30
[mm<sup>3</sup>]; ISO 4649
Compression Set 32 %

@Temperature 23.0 °C,
Time 252000 sec
32 %

@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
50 %

@Temperature 70.0 °C,
Time 86400 sec
50 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 185 - 200 °C
365 - 392 °F
Huntsman/TMA