Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D995
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 42
42
ASTM D2240
Tensile Strength at Break 50.0 MPa
7250 psi
DIN 53504
Elongation at Break 470 %
470 %
ASTM D412
100% Modulus 0.0123 GPa
1.78 ksi
DIN 53504
300% Modulus 0.0308 GPa
4.47 ksi
DIN 53504
Rebound 35 %
35 %
Bayshore; ASTM D2632
Tear Strength 105 kN/m
600 pli
ASTM D624
Abrasion 30
30
[mm<sup>3</sup>]; ISO 4649
Compression Set 29 %

@Temperature 23.0 °C,
Time 252000 sec
29 %

@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
82 %

@Temperature 70.0 °C,
Time 86400 sec
82 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 175 - 188 °C
347 - 370 °F
Huntsman/TMA
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not reported