Huntsman IROGRAN® A 95 P 5003 TPU-Polyether

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® A 95 P 5003 TPU-Polyether.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IROGRAN® A 95 P 5003 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
injection molded; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
Injection molded; ASTM D2240
Hardness, Shore D 41
41
Injection molded; ASTM D2240
Tensile Strength at Break 14.5 MPa
2100 psi
25 mil film; ASTM D412
Elongation at Break 510 %
510 %
25 mil film; ASTM D412
100% Modulus 0.00896 GPa
1.30 ksi
25 mil film; ASTM D412
300% Modulus 0.0110 GPa
1.60 ksi
25 mil film; ASTM D412
Tear Strength 77.1 kN/m
440 pli
25 mil film; ASTM D624
Abrasion 120
120
mm<sup>3</sup>, injection molded; ISO 4649
Thermal Properties Metric English Comments
Melting Point 159 - 174 °C
318 - 345 °F
TMA Melt Range, 25 mil film
Flammability, UL94 V-0
V-0
Oxygen Index 34 %
34 %
injection molded; ASTM D2863