Material Notes:
Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range and offers a specially designed, flexible material with a broad processing window.Performance Features: High wear resistance Medium crystallinity Abrasion resistance Flex resistance Phthalate free TPUApplications: General Injection molding parts Screens Wheels and rollers Shoe solesInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Injection molded parts; ASTM D792
Melt Index of Compound 20 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
Injection molded parts; ASTM D2240
Hardness, Shore D 37
37
Injection molded parts; ASTM D2240
Tensile Strength at Break 50.0 MPa
7250 psi
Injection molded parts; DIN 53504
Elongation at Break 600 %
600 %
Injection molded parts; DIN 53504
100% Modulus 0.00600 GPa
0.870 ksi
Injection molded parts; DIN 53504
300% Modulus 0.0140 GPa
2.03 ksi
Injection molded parts; DIN 53504
Tear Strength 85.0 kN/m
485 pli
Injection molded parts; DIN 53515
Abrasion 20
20
mm<sup>3</sup>, Injection molded; DIN 53516
Processing Properties Metric English Comments
Nozzle Temperature 185 - 195 °C
365 - 383 °F
Injection
Zone 1 87.8 - 93.3 °C
190 - 200 °F
Zone 2 90.6 - 96.1 °C
195 - 205 °F
Zone 3 93.3 - 98.9 °C
200 - 210 °F
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Injection