Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Manufactures of technical parts can achieve the highest levels of: Wear and tear strengthDimensional stabilityOil resistanceLow compression setDynamic load performanceElasticity and flexibilityTemperature performanceProcessing consistencyInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Linear Mold Shrinkage 0.030 cm/cm
0.030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Hardness, Shore D 18
18
ASTM D2240
Tensile Strength at Break 25.5 MPa
3700 psi
ASTM D412
Elongation at Break 900 %
900 %
ASTM D412
100% Modulus 0.00352 GPa
0.510 ksi
ASTM D412
300% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Rebound 54 %
54 %
Bayshore; ASTM D2632
Tear Strength 63.1 kN/m
360 pli
ASTM D624
Abrasion 55
55
mm<sup>3</sup>; ISO 34-1
Compression Set 43 %

@Temperature 22.8 °C,
Time 252000 sec
43 %

@Temperature 73.0 °F,
Time 70.0 hour
ASTM D395
54 %

@Temperature 70.0 °C,
Time 86400 sec
54 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 140 - 170 °C
284 - 338 °F
TMA Melt Range