Huntsman HY 265 Cycloaliphatic Amine

Category Polymer , Thermoset , Epoxy , Epoxy, Cycloaliphatic, Molded
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman HY 265 Cycloaliphatic Amine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Approx. H+ equivalent weight 94. Mix Ratio with GY 6010 is 50.Comments/Applications: Modified cycloaliphatic polyamine adduct. Excellent chemical resistance. Exceptional sulfuric acid (96-98%) resistance. High performance solvent free coatings for chemical storage tanks and chemical process equipment.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 2700 - 10000 cP
2700 - 10000 cP
Processing Properties Metric English Comments
Pot Life 40 min
40 min