Huntsman DY 9577 Special Hardener

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman DY 9577 Special Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix Ratio with 100 phr GY 6010 is 1.Comments/Applications: Latent catalytic curing agent for liquid epoxy resins or as a latent accelerator for anhydride cured epoxy resins. Latent at RT in GY 6010. BCL3 amine complex. Yellowish brown semi-solid. High reactivity above 120°C. Good working time below 80°C. Casting, encapsulation, powder coatings, filament winding, pultrusion, molding, electrical tapes.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 25.0 - 31.0 °C
77.0 - 87.8 °F
Softening Range
Processing Properties Metric English Comments
Processing Temperature 120 °C
248 °F
Cure Schedule: 2 hrs @ 120ºC, 6 hrs @ 150°C, or 2 hrs @ 190°C