Huntsman DY 062 Epoxy Accelerator

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman DY 062 Epoxy Accelerator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix Ratio with GY 6010 is 5.Comments/Applications: Reduces gel time and cure schedule for adhesives and other fast cure epoxy systems. Benzyl dimethyl amine (BDMA)-tertiary amine accelerator. Compatible with anhydride and polyamide hardeners. Flexible mix ratio = 0.5 - 10.0 PHR, with GY 6010.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1.0 - 5.0 cP
1.0 - 5.0 cP