Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman AroCy M-10 Monomeric Bisphenol F Dicyanate

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name AroCy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman AroCy M-10 Monomeric Bisphenol F Dicyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Comments/Applications: Very hydrophobic after cure. Monomeric tetramethyl bisphenol F dicyanate. Low viscosity impregnations.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 103 - 108 °C
217 - 226 °F
Softening Range
Copyright © lookpolymers.com All Rights Reserved