Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman AroCy B-40S Prepolymer Bisphenol-A Dicyanate

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name AroCy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman AroCy B-40S Prepolymer Bisphenol-A Dicyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Comments/Applications: Prepolymer of high purity bisphenol A dicyanate supplied @ 75% solids in MEK. High performance multi-layer printed wiring boards and multi-chip modules.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 200 - 375 cP
200 - 375 cP
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved