Huntsman Araldite GY 9667 Bisphenol A Epoxy Liquid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GY 9667 Bisphenol A Epoxy Liquid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 196 to 212. Max color is 2.Comments/Applications: GY 6020 modified with DY 025 (Epoxide 8) for less crystallization and improved elongation. High solids and solvent free coatings and floorings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 500 - 700 cP
500 - 700 cP