Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman Araldite GY 502 Bisphenol A Epoxy Liquid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GY 502 Bisphenol A Epoxy Liquid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 222 to 238. Max color is 3.Comments/Applications: GY 6010 modified with dibutyl phthalate - a non-reactive diluent. Increases resiliency of cured product; suitable for low temperature applications.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 2100 - 3600 cP
2100 - 3600 cP