Huntsman Araldite GT 6243 Bisphenol A Epoxy Solid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GT 6243 Bisphenol A Epoxy Solid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 1200 to 1400. Max color is 3.Comments/Applications: Unmodified bis A "Type 6" epoxy resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 - 120 °C
230 - 248 °F
Softening Range