Huntsman Araldite EPN 1138 Epoxy Phenol Novolac

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite EPN 1138 Epoxy Phenol Novolac.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 176 to 181. Max color is 2.Comments/Applications: Epoxy phenol novolac for higher heat and chemical resistance than PY 307-1 and EPN 1139 or EPN 1179. Used in coatings and composites applications including filament winding, casting and pultrusion. Epoxy functionality of 3.6. Much higher viscosity than EPN 1139.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 20000 - 50000 cP
20000 - 50000 cP