Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman Araldite ECN 1273 Epoxy Cresol Novolac

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite ECN 1273 Epoxy Cresol Novolac.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 217 to 233. Max color is
Physical Properties Metric English Comments
Viscosity 68 - 78 cP
68 - 78 cP
Copyright © lookpolymers.com All Rights Reserved