Hong Kun Group DBDPE Flame Retardant

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group DBDPE Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name:1,2-Bis(pentabromophenyl) ethaneDecabromodiphenylethaneDecabromodiphenyl EthylCAS No. 84852-53-9All information provided by Hongkun Group
Physical Properties Metric English Comments
Particle Size <= 2.0 µm
<= 2.0 µm
Thermal Properties Metric English Comments
Melting Point >= 340 °C
>= 644 °F
Descriptive Properties Value Comments
Appearance white powder
Bromide Content (%) >= 81.5
Whiteness >= 88