Hong Kun Group AO 168 Antioxidant

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group AO 168 Antioxidant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAS No. 31570-04-4All information provided by Hongkun Group
Physical Properties Metric English Comments
Evaporation Loss <= 0.30 %
<= 0.30 %
loss on drying
Thermal Properties Metric English Comments
Melting Point 183 - 187 °C
361 - 369 °F
Optical Properties Metric English Comments
Transmission, Visible >= 97 %

@Wavelength 425 nm
>= 97 %

@Wavelength 425 nm
>= 98 %

@Wavelength 500 nm
>= 98 %

@Wavelength 500 nm
Descriptive Properties Value Comments
Appearance white powder
Purity (%) >= 99