Hong Kun Group 2,2,6,6-Tetramethyl-piperidine-1-oxyl(TEMPO) Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group 2,2,6,6-Tetramethyl-piperidine-1-oxyl(TEMPO) Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UN3263 Hazard class 8 PG IICAS No. 2564-83-2All information provided by Hongkun Group
Physical Properties Metric English Comments
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 34.0 - 38.0 °C
93.2 - 100 °F
Descriptive Properties Value Comments
Appearance hyacinth solid or liquid
Purity (%) >= 98.0
GC