Honeywell Spectra® 1000 Fiber

Category Other Engineering Material , Composite Fibers , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Honeywell
Trade Name Spectra®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Spectra® 1000 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Spectra® fiber 1000, the second in a series of Spectra® fibers, was developed to meet customers’ needs for increased performance. It is available in a multitude of deniers for use in a wide range of applications. This extended chain polyethylene fiber has one of the highest strength to weight ratios of any manmade fiber. Spectra® fiber 1000 has a tenacity 15 – 20 percent higher than that of Spectra® fiber 900. Spectra® fiber is, pound-for-pound, 10 times stronger than steel, more durable than polyester and has a specific strength that is 40 percent greater than aramid fiber. Specific performance is dependent upon denier and filament count.  Spectra® is a registered trademark of Honeywell and was formerly a product of Allied Signal.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3000 MPa
435000 psi
Modulus of Elasticity 172 GPa
24900 ksi
Thermal Properties Metric English Comments
Melting Point 147 °C
297 °F