Honeywell PMP Polymethylpentene Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polymethylpentene (PMP) , Polymethylpentene, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell PMP Polymethylpentene Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
Density 0.913 g/cc
0.0330 lb/in³
Yield Density
Water Vapor Transmission 46.5 g/m²/day
2.99 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Thickness 49.5 microns
1.95 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 - 210 %
150 - 210 %
ASTM D882
Film Elongation at Break, TD 380 - 500 %
380 - 500 %
ASTM D882
Secant Modulus, MD 0.552 - 0.648 GPa
80.1 - 94.0 ksi
ASTM D882
Secant Modulus, TD 0.621 - 0.703 GPa
90.1 - 102 ksi
ASTM D882
Coefficient of Friction 0.50 - 0.70
0.50 - 0.70
film to stainless steel; ASTM D1894
0.80 - 1.2
0.80 - 1.2
film to film; ASTM D184
Tear Strength Test 220 - 280
220 - 280
graves tear MD, grams/mil; ASTM D1004
220 - 280
220 - 280
graves tear TD, grams/mil; ASTM D1004
Film Tensile Strength at Break, MD 39.3 - 53.1 MPa
5700 - 7700 psi
ASTM D882
Film Tensile Strength at Break, TD 21.4 - 39.3 MPa
3100 - 5700 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD <= 2.0 %
<= 2.0 %
350°F / 177°C - 10 min.; ASTM D1204
Shrinkage, TD <= 1.5 %
<= 1.5 %
350°F / 177°C - 10 min.; ASTM D1204
Copyright © lookpolymers.com All Rights Reserved