Honeywell Capran® NyLid™ WMB 175 Nylon Lidding Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Alcohol (EVOH) , Nylon
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Capran® NyLid™ WMB 175 Nylon Lidding Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Capran® NyLid™ WMB 175 is a 1.75 mil, white medium barrier nylon co-extruded film with an EVOH core. Applications: Capran® NyLid™ WMB 175 is suitable for die cutting, readily accepts printing, accepts heal seal coatings and lacquers, offers excellent puncture resistance, is safe for microwave use, and resists tear propagation. It is ideally suited for lamination, and is FDA compliant for indirect food contact.Information provided by Honeywell.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0420 lb/in³
Yield Density
Water Vapor Transmission 217.1 g/m²/day
13.98 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Oxygen Transmission Rate 1.40 cc/m²/day
0.0902 cc/100 in²/day
ASTM D3985
Thickness 44.5 microns
1.75 mil
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 34.5 MPa
5000 psi
ASTM D882
Film Tensile Strength at Yield, TD 34.5 MPa
5000 psi
ASTM D882
Film Elongation at Break, MD 360 %
360 %
ASTM D882
Film Elongation at Break, TD 370 %
370 %
ASTM D882
Secant Modulus, MD 1.027 GPa
149.0 ksi
ASTM D882
Secant Modulus, TD 0.9997 GPa
145.0 ksi
ASTM D882
Coefficient of Friction 0.21
0.21
film to stainless steel; ASTM D1894
0.40
0.40
film to film; ASTM D184
Tear Strength Test 520
520
graves tear MD, initial, grams/mil; ASTM D1004
520
520
graves tear TD, initial, grams/mil; ASTM D1004
Elmendorf Tear Strength, MD 4.500 g/micron
114.3 g/mil
Elmendorf Tear Strength, TD 6.7492 g/micron
171.43 g/mil
propagated; ASTM D1922
Film Tensile Strength at Break, MD 101 MPa
14700 psi
ASTM D882
Film Tensile Strength at Break, TD 89.6 MPa
13000 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD -3.20 %
-3.20 %
350°F / 177°C - 10 min.; ASTM D1204
Shrinkage, TD >= -0.600 %
>= -0.600 %
350°F / 177°C - 10 min.; ASTM D1204
Optical Properties Metric English Comments
Gloss 80 %
80 %
at 60°; ASTM D2457