Material Notes:
Description: Capran® 996 is a blue tinted, heat-stabilized cast film produced from modified nylon resin. Capran® 996 has excellent heat stability and resistance to pinholing. It can be used at temperatures up to 450°F (232°C) for typical cure cycle times. Applications: Capran® 996 is recommended as bagging film for advanced composite fabrication and other high temperature applications where softness and workability are essential. Information provided by Honeywell.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0410 lb/in³
Yield Density
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D882
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D882
Elongation at Break 300 %
300 %
ASTM D882
Tear Strength Test 30
30
grams/mil; ASTM D1922
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
crystalline melting point; Hot Stage Microscope
Shrinkage <= 1.00 %

@Temperature 149 °C,
Time 1800 sec
<= 1.00 %

@Temperature 300 °F,
Time 0.500 hour
ASTM D1204