Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal , Copper Alloy , Refractory Metal , Tungsten Alloy
Manufacturer Hogen Industries
Trade Name Duralloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection welding dies requiring low pressure. Another common use is tips on contact shoe facings used in high frequency continuous welding processes. Same general uses as Hogen H5W, but with higher wear resistance.Data provided by Hogen Industries.
Physical Properties Metric English Comments
Density >= 11.0 g/cc
>= 0.397 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Tensile Strength, Ultimate 483 MPa
70100 psi
Thermal Properties Metric English Comments
CTE, linear 12.2 µm/m-°C

@Temperature 20.0 °C
6.78 µin/in-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Copper, Cu 50 %
50 %
WC 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000370 ohm-cm
0.00000370 ohm-cm