Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hogen Duralloy H10TC 56 Tungsten Carbide/44 Copper PM Metal Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Hogen Industries
Trade Name Duralloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hogen Duralloy H10TC 56 Tungsten Carbide/44 Copper PM Metal Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for heavy-duty or projection welding electrodes where the pressures involved are relatively high and for die facings in electro-forming and electro-forging applications. It is suitable as die material for electrical upsetting of non-ferrous metals and low carbon steel or for cross-wire welding of larger diameter wire and rod. Same general uses as Hogen H30W, but with higher wear resistance.Data provided by Hogen Industries.
Physical Properties Metric English Comments
Density >= 11.3 g/cc
>= 0.408 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 95
95
Tensile Strength, Ultimate 517 MPa
75000 psi
Thermal Properties Metric English Comments
CTE, linear 11.5 µm/m-°C

@Temperature 20.0 °C
6.39 µin/in-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Copper, Cu 44 %
44 %
WC 56 %
56 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000420 ohm-cm
0.00000420 ohm-cm