Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.90 g/cc
1.50 - 1.90 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Flexural Strength >= 250 MPa
>= 36300 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 10.0 GPa
>= 1450 ksi
IEC 1212-2 5.2
Compressive Strength >= 250 MPa
>= 36300 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 20.0 MPa
>= 2900 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 44.0 kJ/m²
>= 20.9 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 5.00 J/cm²
>= 23.8 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+8 ohm
>= 5.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 4.5

@Frequency 48.0 - 62.0 Hz
<= 4.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 4.5

@Frequency 1.00e+6 Hz
<= 4.5

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 35000 V

@Temperature 90.0 °C
>= 35000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050

@Frequency 48.0 - 62.0 Hz
<= 0.050

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.050

@Frequency 1.00e+6 Hz
<= 0.050

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 600 V
>= 600 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Proof Tracking Index 500
IEC 1212-2 6.4
Thermal Endurance 140 T.I.
IEC 1212-2 7.1
Water Absorption < 101 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm