Hippe PS Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PS Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amorphous thermoplastic with brilliant surface. High hardness and stiffness, but brittle and susceptible to impact. Very good dielectric properties. Physiologically safe if it falls below a particular value of monomer content.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
DIN 53 479
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
Absorption of humidity in standard operating environment; DIN 53 715
Mechanical Properties Metric English Comments
Ball Indentation Hardness 150 MPa

@Time 30.0 sec
21800 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 45.0 MPa
6530 psi
DIN 53 455
Elongation at Break 3.0 %
3.0 %
DIN 53 455
Tensile Modulus 3.20 GPa
464 ksi
DIN 53 457
Flexural Modulus 3.20 GPa
464 ksi
from bending test; DIN 53 457
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
DIN 53 453
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 70.0 °C
158 °F
Continuous use
80.0 °C
176 °F
Short Periods
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO-R 75 Method A
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
DIN 53 482
Dielectric Constant 2.5

@Frequency 1.00e+6 Hz
2.5

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 60.0 kV/mm
1520 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.00040

@Frequency 1.00e+6 Hz
0.00040

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Creep Resistance Grade CTI 350
DIN 53 480, IEC-112, VDE 0303 Part 1