Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet

Category Polymer , Thermoset , Phenolic , Phenolic/Glass Fiber SMC
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Flexural Strength >= 400 MPa
>= 58000 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 22.0 GPa
>= 3190 ksi
IEC 1212-2 5.2
Compressive Strength >= 400 MPa
>= 58000 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 35.0 MPa
>= 5080 psi
Parallel to laminations; IEC 1212-2 5.6
Charpy Impact Unnotched >= 7.00 J/cm²
>= 33.3 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
IEC 1212-2 7.2
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+8 ohm
>= 1.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.5

@Frequency 48.0 - 62.0 Hz
<= 5.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 5.5

@Frequency 1.00e+6 Hz
<= 5.5

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 40000 V

@Temperature 90.0 °C
>= 40000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.030

@Frequency 48.0 - 62.0 Hz
<= 0.030

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.030

@Frequency 1.00e+6 Hz
<= 0.030

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 150 V
>= 150 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 160 T.I.
IEC 1212-2 7.1
Water Absorption < 127 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm