Material Notes:
Used in electronic applications. Good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.40 g/cc
1.30 - 1.40 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 80.0 MPa
>= 11600 psi
IEC 1212-2 5.7
Flexural Strength >= 110 MPa
>= 16000 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 6.00 GPa
>= 870 ksi
IEC 1212-2 5.2
Compressive Strength >= 160 MPa
>= 23200 psi
Perpendicular to laminations; IEC 1212-2 5.3
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
IEC 1212-2 7.2
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+10 ohm
>= 1.00e+10 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.0

@Frequency 48.0 - 62.0 Hz
<= 5.0

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 5.0

@Frequency 1.00e+6 Hz
<= 5.0

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 20000 V

@Temperature 90.0 °C
>= 20000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050

@Frequency 48.0 - 62.0 Hz
<= 0.050

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.050

@Frequency 1.00e+6 Hz
<= 0.050

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 100 V
>= 100 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 110 T.I.
IEC 1212-2 7.1