Material Notes:
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A supported version, Redux® 312/5, is available with a woven nylon carrier for bond line thickness control.Features: Short cure cycle - cures in 30 minutes at 250°F; Good mechanical performance up to 210°F; Suitable for composite to composite bonding; Low volatile content (solventless process).Applications: Metal to metal bonding; Sandwich constructions; Composite to composite bonding.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.10 MPa

@Temperature 21.1 °C
1320 psi

@Temperature 70.0 °F
Flatwise Tensile
Shear Strength 29.6 MPa

@Temperature 98.9 °C
4300 psi

@Temperature 210 °F
Lap Shear
39.3 MPa

@Temperature 71.1 °C
5700 psi

@Temperature 160 °F
Lap Shear
42.7 MPa

@Temperature 21.1 °C
6200 psi

@Temperature 70.0 °F
Lap Shear
Peel Strength 9.12 kN/m

@Temperature 21.1 °C
52.0 pli

@Temperature 70.0 °F
Bell Peel
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Areal Weight (psf) 0.06
Climbing Drum Peel (in-lb/3in) 80
70°F
Roll Width (in) 21
Standard Roll (ft2) 645