Hexcel® HexWeb® HRH-78 - 1/8 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin

Category Polymer , Thermoset , Phenolic
Manufacturer Hexcel
Trade Name HexWeb®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-78 - 1/8 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding, the block is dipped in a phenolic resin. After curing the resin, slices are cut to the desired thickness. Using this process, a wide range of cell sizes, paper thicknesses, and densities can be produced. An OX-Core confiation featuring enhanced formability is available upon request.Features: High strength at low densities; Small cell sizes at low densities; Damage resistant under normal shop use; Formable; Flame resistant; Good bonding surfaces; Good thermal and electrical insulator.Applications: HexWeb HRH-78 was developed by Hexcel to offer most of the characteristics of HexWeb HRH-10 for exclusive use in non-aerospace applications, such as pleasure boats, skis, surfboards, ground antennas, and navy joiner panels.
Physical Properties Metric English Comments
Density 0.0481 g/cc
0.00174 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength 1.93 MPa
280 psi
Bare
2.17 MPa
315 psi
Stabilized
Compressive Modulus 0.128 GPa
18.5 ksi
Stabilized, preliminary value obtained from limited testing
Shear Modulus 0.0214 GPa
3.10 ksi
Plate Shear, W Direction, preliminary value obtained from limited testing
0.0365 GPa
5.30 ksi
Plate Shear, L Direction, preliminary value obtained from limited testing
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, W Direction
1.10 MPa
160 psi
Plate Shear, L Direction