Hexcel® HexWeb® HRH-36 - 1/8 - 4.0 Para-Aramid/Phenolic Core

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Aramid , Phenolic
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-36 - 1/8 - 4.0 Para-Aramid/Phenolic Core.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low moisture pickup; Excellent thermal stability; Smooth cell wall finish.Applications: HexWeb® HRH-36 is a high performance non-metallic core, available in a wide range of densities, suitable for most composite sandwich applications. It can be readily heat formed to help produce complex components and offers similar mechanical properties to KOREX® core as well as comparable moisture pickup. In addition, HexWeb® HRH-36 offers a weight reduction over higher density NOMEX® honeycomb cores.
Physical Properties Metric English Comments
Density 0.0641 g/cc
0.00231 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength 3.28 MPa
475 psi
Bare
4.03 MPa
585 psi
Stabilized
Shear Modulus 0.0607 GPa
8.80 ksi
Plate Shear, W Direction
0.106 GPa
15.4 ksi
Plate Shear, L Direction
Shear Strength 1.17 MPa
170 psi
Plate Shear, W Direction
1.90 MPa
275 psi
Plate Shear, L Direction