Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb

Category Metal , Metal Foam, Mesh, or Honeycomb , Nonferrous Metal , Aluminum Alloy , 5000 Series Aluminum Alloy
Manufacturer Hexcel
Trade Name HexWeb®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the face sheets that carry bending loads and the honeycomb that carries the shear loads. The adhesive is the interface between the facing and the core in the same way that the oxide on the aluminum and the primer that has been applied to it is the interface between the honeycomb substrate material and the bonding adhesive. This interface is critical to the performance of honeycomb bonded assemblies.HexWeb® CR-PAA™ is designed for aircraft structures that are exposed to demanding environmental conditions. HexWeb® CR-PAA™ outperforms standard MIL-C-7438 core in salt spray and HexWeb® crack propagation tests.
Physical Properties Metric English Comments
Density 0.0497 g/cc
0.00179 lb/in³
Nominal
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 1.38 MPa
>= 200 psi
Bare, min
>= 1.48 MPa
>= 215 psi
Stabilized, min
2.00 MPa
290 psi
Bare, typ
2.31 MPa
335 psi
Stabilized, typ
Compressive Modulus 0.517 GPa
75.0 ksi
Stabilized, typ
Shear Modulus 0.152 GPa
22.0 ksi
Plate Shear, W Direction, typ
0.310 GPa
45.0 ksi
Plate Shear, L Direction, typ
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min
0.862 MPa
125 psi
Plate Shear, W Direction, typ
>= 1.07 MPa
>= 155 psi
Plate Shear, L Direction, min
1.45 MPa
210 psi
Plate Shear, L Direction, typ