Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Cured Resin
1.77 g/cc
0.0639 lb/in³
Nominal Laminate
2.54 g/cc
0.0918 lb/in³
Fibre
Mechanical Properties Metric English Comments
Tensile Strength, Yield 470 MPa
68200 psi
EN2597B
Tensile Modulus 25.0 GPa
3630 ksi
EN2597B
Shear Strength 67.0 MPa
9720 psi
ILSS; EN2563
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 211 °C
412 °F
EN6032
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0269
Fiber Volume (%) 44
Nominal
Users viewing this material also viewed the following: