Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 600 g/m2

Category Polymer , Thermoset , Epoxy , Epoxy/Glass SMC
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, E-glass Balanced Fabric 600 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 400 MPa
58000 psi
Tensile Modulus 20.0 GPa
2900 ksi
Flexural Yield Strength 670 MPa
97200 psi
Flexural Modulus 20.0 GPa
2900 ksi
Shear Strength 53.0 MPa
7690 psi
0º, Short Beam
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Fiber Volume (%) 50