Hexcel® HexPly® F593 Epoxy Resin, W3T282 Carbon Fabric

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F593 Epoxy Resin, W3T282 Carbon Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: W3T282-42"-F593; Fiber: Toray T-300/3kInformation provided by HexCel
Physical Properties Metric English Comments
Volatiles 1.0 - 6.0 %
1.0 - 6.0 %
Prepreg
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.021-0.024
Laminate
Dry Resin Content (%) 38-46
Prepreg
Fiber Volume (%) 45-53
Laminate
Flow (%) <4.5