Hexcel® HexPly® F522 Epoxy Resin, T_095 Carbon Tape

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F522 Epoxy Resin, T_095 Carbon Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: T_095-12"-F522; Various Fibers; (95 g/m2)Information provided by HexCel
Descriptive Properties Value Comments
Dry Resin Content (%) 37-41
Prepreg
Fiber Volume (%) 0.009
Laminate
Flow (%) 4-16
Wet Resin Content (%) 52
Laminate