Hexcel® HexPly® F522 Epoxy Resin, 1581 Glass Fabric

Category Polymer , Thermoset , Epoxy , Epoxy/Glass SMC
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F522 Epoxy Resin, 1581 Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: 1581-38"-F522; Fiber: 150-1/2Information provided by HexCel
Descriptive Properties Value Comments
Dry Resin Content (%) 37-43
Prepreg
Fiber Volume (%) 0.036
Laminate
Flow (%) 16-28
Wet Resin Content (%) 45
Laminate