Material Notes:
Hexcel designation: T_190-12"-F263; Various fibersInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1353 MPa

@Temperature 24.0 °C
196200 psi

@Temperature 75.2 °F
Tensile Modulus 131.8 GPa

@Temperature 24.0 °C
19120 ksi

@Temperature 75.2 °F
Compressive Yield Strength 1185 MPa

@Temperature 71.0 °C
171900 psi

@Temperature 160 °F
1212 MPa

@Temperature 24.0 °C
175800 psi

@Temperature 75.2 °F
Shear Strength 76.0 MPa

@Temperature 132 °C
11000 psi

@Temperature 270 °F
Short Beam
110 MPa

@Temperature 24.0 °C
16000 psi

@Temperature 75.2 °F
Short Beam
122 MPa

@Temperature -54.0 °C
17700 psi

@Temperature -65.2 °F
Short Beam
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.02
Laminate
Dry Resin Content (%) 35-39
Prepreg
Fiber Volume (%) 55
Laminate
Flow (%) 11-24