Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel
Physical Properties Metric English Comments
Volatiles 0.40 - 1.2 %
0.40 - 1.2 %
Prepreg
Mechanical Properties Metric English Comments
Tensile Strength, Yield 440 MPa

@Temperature 24.0 °C
63800 psi

@Temperature 75.2 °F
Warp TS
Compressive Yield Strength 324 MPa

@Temperature 24.0 °C
47000 psi

@Temperature 75.2 °F
Warp compression
Shear Strength 20.278 MPa

@Temperature 82.0 °C
2941.1 psi

@Temperature 180 °F
Lap shear
31.757 MPa

@Temperature 24.0 °C
4606.0 psi

@Temperature 75.2 °F
Lap shear
32.737 MPa

@Temperature -54.0 °C
4748.1 psi

@Temperature -65.2 °F
Lap shear
Peel Strength 5.65 kN/m

@Temperature -54.0 °C
32.2 pli

@Temperature -65.2 °F
Metal-to-metal
13.4 kN/m

@Temperature 24.0 °C
76.5 pli

@Temperature 75.2 °F
Metal-to-metal
13.4 kN/m

@Temperature 82.0 °C
76.5 pli

@Temperature 180 °F
Metal-to-metal
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.021
Laminate
Fiber Volume (%) 56
Laminate
Flow (%) 24-34
Wet Resin Content (%) 47-53
Prepreg