Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 400 MPa
58000 psi
Tensile Modulus 35.0 GPa
5080 ksi
Flexural Yield Strength 450 MPa
65300 psi
Flexural Modulus 35.0 GPa
5080 ksi
Shear Strength 40.0 MPa
5800 psi
0°, Short Beam
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30